    Effect of sintering on the physical and mechanical properties of Co-Cr-Mo (F-75)/HAP composites

    Thumbnail
    View/Open
    Effect of sintering on the physical and mechanical properties of Co-Cr-Mo (F-75)-HAP composites.pdf (12.04Kb)
    Date
    2013-12
    Author
    Nur Maizatul Shima, Adzali, Dr.
    Shamsul Baharin, Jamaludin, Prof. Dr.
    Mohd. Nazree, Derman, Dr.
    Metadata
    Show full item record
    Abstract
    This paper reports on the effects of HAP addition and sintering temperature on the microstructure and properties of the F-75/HAP composites fabricated by powder metallurgy. Co-Cr-Mo (F-75) is used in orthopedics because of its excellent biocompatibility when implanted to human or animal body. Hydroxyapatite (HAP) powders have been used as fillers because HAP is the one of the most effective biocompatible materials with similarities to mineral constituents of bones and teeth. HAP powders (chemical formula Ca 10(PO4)6 (OH)2) have been added to Co-Cr-Mo alloys in composition of 0 to 10 wt. %. The mixtures were then milled, cold compacted at 550 MPa, before sintered at 1100 and 1200°C in a tube furnace. The density, porosity, microhardness and compressive strength were measured. The composites that have been sintered at temperature 1200°C showed better physical and mechanical properties than those produced at 1100°C. After sintering at 1200°C, the samples show higher density, compared with the sample sintered at 1100°C. The sample with no HAP which have been sintered at 1200°C has the highest microhardness (208.9 HV), compared with the same sample sintered at 1100°C (194.3HV). As the temperature is increased from 1100 to 1200°C, the value of compressive strength increased from 184.538 to 341.086 MPa. Microstructural analysis for line scan showed that, as the sintering temperature was increased, there was good interface bonding between HAP particles and matrix F-75.
    URI
    http://www.ukm.my/jsm/english_journals/vol42num12_2013/contentsVol42num12_2013.html
    http://dspace.unimap.edu.my:80/dspace/handle/123456789/32215
    Collections
    • Mohd Nazree Derman, Assoc. Prof. Dr. [66]
    • Shamsul Baharin Jamaludin, Prof. Dr. [87]
    • School of Materials Engineering (Articles) [553]
    • Institute of Nano Electronic Engineering (INEE) (Articles) [206]

    Atmire NV

    Perpustakaan Tuanku Syed Faizuddin Putra (PTSFP) | Send Feedback
     

     

    Browse

    All of UniMAP Library Digital RepositoryCommunities & CollectionsBy Issue DateAuthorsTitlesSubjectsThis CollectionBy Issue DateAuthorsTitlesSubjects

    My Account

    LoginRegister

    Statistics

    View Usage Statistics

    Atmire NV

    Perpustakaan Tuanku Syed Faizuddin Putra (PTSFP) | Send Feedback