Show simple item record

dc.contributor.authorMohd Mustafa Al Bakri, Abdullah
dc.contributor.authorKamarudin, Hussin, Brig. Jen. Dato' Prof. Dr.
dc.contributor.authorO. A. K. A., Karem
dc.contributor.authorChe Mohd Ruzaidi, Ghazali, Prof. Madya
dc.contributor.authorRafizah, Abu Rashid
dc.contributor.authorNorazian, Mohamed Noor
dc.date.accessioned2012-04-10T08:11:29Z
dc.date.available2012-04-10T08:11:29Z
dc.date.issued2012
dc.identifier.citationApplied Mechanics and Materials, vol. 110-116, 2012, pages 734-739en_US
dc.identifier.isbn978-3-0378-5262-0
dc.identifier.issn1660-9336
dc.identifier.urihttp://www.scientific.net/AMM.110-116.734
dc.identifier.urihttp://dspace.unimap.edu.my/123456789/18749
dc.descriptionLink to publisher's homepage at http://www.ttp.net/en_US
dc.description.abstractFly ash and a mixture of alkaline activators namely sodium silicate (Waterglass) and sodium hydroxide (NaOH) solution were used for preparing geopolymer. The aim of this research is to determine the optimum value of the alkaline activator/fly ash ratio. The effect of the oxide molar ratios of SiO2/Al2O3, water content of the alkaline activator and the Waterglass% content were studied for each Alkaline activator/fly ash ratio. The geopolymers were synthesized by the activation of fly ash with alkaline solution at three different alkaline activator/fly ash ratios which were 0.3, 0.35, and 0.4 at a specific constant ratio of waterglass/NaOH solution of 1.00. The geopolymers were cured at 70°C for 24 h and cured to room temperature. Results revealed that the alkaline activator/fly ash ratio of 0.4 has the optimum amount of alkaline liquid, which shows the highest rate of geopolymerization compared to other ratios. A high strength of 8.61 MPa was achieved with 0.4 of activator/fly ash ratio and 14% of waterglass content.en_US
dc.language.isoenen_US
dc.publisherTrans Tech Publicationsen_US
dc.subjectAlkaline activator / fly ash ratioen_US
dc.subjectCompressive strengthen_US
dc.subjectGeopolimerizationen_US
dc.subjectGeopolymeren_US
dc.titleOptimization of alkaline activator / fly ash ratio on the compressive strength of manufacturing fly ash-based geopolymeren_US
dc.typeArticleen_US