dc.description.abstractThe hot corrosion behaviour of Nickel-200 industrial alloy has been investigated in presence of Na2S04, NaCI, NaN03, Na2C03 and Na202 at 850°C in flowing air. The hot corrosion kinetic and effect of salt deposition on the corrosion rate were studied. The scale morphologies were determined on the basis of X-ray diffraction and Scanning electron microscopic techniques. It has been shown that an alloy corrodes at different rate in presence of different sodium salts although each salt contains the same amount of sodium equivalent to Na20.en_US
dc.language.isoenen_US
dc.publisherAcademy Science Publishers/African Academy of Sciences (AAS)en_US
dc.subjectAlloysen_US
dc.subjectIndustrial alloyen_US
dc.subjectCorrosionen_US
dc.subjectHot corrosionen_US
dc.subjectNickel alloysen_US
dc.subjectSEMen_US
dc.subjectHeat resistant alloysen_US
dc.subjectNickel alloys -- Thermal propertiesen_US
dc.titleHot corrosion behaviour of Nickel-200 alloy in presence of Sodium salts at 850°Cen_US
dc.typeArticleen_US
dc.publisher.departmentFaculty of Science, University of Maiduguri, Nigeriaen_US


Files in this item

Thumbnail

This item appears in the following Collection(s)

Show simple item record