dc.contributor.author | Mohammed Misbahul, Amin | |
dc.date.accessioned | 2009-06-26T03:02:28Z | |
dc.date.available | 2009-06-26T03:02:28Z | |
dc.date.issued | 1994 | |
dc.identifier.citation | Thin Solid Films, vol. 237 (1-2), 1994, pages 172-174. | en_US |
dc.identifier.issn | 0040-6090 | |
dc.identifier.uri | http://www.sciencedirect.com/science/journal/00406090 | |
dc.identifier.uri | http://www.sciencedirect.com/science?_ob=ArticleURL&_udi=B6TW0-46SWRXP-R4&_user=1659113&_coverDate=01%2F01%2F1994&_alid=940293886&_rdoc=2&_fmt=high&_orig=search&_cdi=5548&_docanchor=&view=c&_ct=2&_acct=C000054070&_version=1&_urlVersion=0&_userid=1659113&md5=1b09f04518549f44a70bca5923c9a8df | |
dc.identifier.uri | http://dspace.unimap.edu.my/123456789/6254 | |
dc.description | Link to publisher's homepage at http://www.elsevier.com/wps/find/homepage.cws_home | en_US |
dc.description.abstract | The high temperature oxidation behaviour of AISI-304 austenitic steel was studied in the presence of Na2S04, Fe2(S04)3 or a mixture at 973 K in flowing air. The studies were carried out to examine the influence of eutectic and solid phases present in the Na2S04 + Fe2(S04)3 systems on the hot corrosion of AISI-304 steel which is extensively employed as a high temperature structural alloy. The scale morphologies were determined on the basis of X-ray diffraction analysis and scanning electron microscopy. | en_US |
dc.language.iso | en | en_US |
dc.publisher | Elsevier Science B.V. | en_US |
dc.subject | Oxidation | en_US |
dc.subject | Austenitic steel | en_US |
dc.subject | Steel | en_US |
dc.subject | Corrosion | en_US |
dc.subject | Hot corrosion | en_US |
dc.subject | Alloys | en_US |
dc.subject | Steel -- Heat treatment | en_US |
dc.title | Oxidation behaviour of AISI-304 steel in the presence of Na2S04 and Fe2(S04)3 at 973 K | en_US |
dc.type | Article | en_US |