The effects of tensile and morphological properties of styrene butadiene rubber/virgin chloroprene rubber blends (SBR/CRv) and styrene butadiene rubber/recycled chloroprene rubber blends (SBR/CRr) were investigated. The range size of CRr used in this study was 0.3 - 0.7 mm. Both SBR/CRv blends and SBR/CRr blends were prepared using two roll mill at room temperature with blend ratios 95/5, 85/15, 75/25, 65/35 and 50/50. It can be observed that, cure characteristics of SBR/CRr blends have lower cure time, t90 than SBR/ CRv blends.SBR/CRr blends showed higher scorch time, t2 and minimum torque (ML) compared to SBR/CRv blends at all blend ratios compared with the SBR/CRv blends. However, maximum torque (MH) of SBR/CRr blends exhibit the opposite trend compared with the SBR/CRv blends. It can be observed that, the tensile strength and elongation at break of SBR/CRr blends show higher value than SBR/CRv blends particularly up to 15 phr of CRr in the blends. However, SBR/CRr blends shows higher value of tensile modulus (M100) than SBR/CRv blends at all blend ratios. The scanning electron microscopy (SEM) of tensile fracture surface of SBR/CRr blends at 50 blend ratios illustrated a better adhesion and dispersion in comparison with SBR/CRv blends.
URI
http://www.revmaterialeplastice.ro/article_eng.asp?ID=3791http://dspace.unimap.edu.my:80/dspace/handle/123456789/32808
Collections
Related items
Showing items related by title, author, creator and subject.
-
The influences of tor as a compatibilizer on cure characteristic and morphological properties of SBR/CRr blends
Ahmad Azrem, Azmi; Nik Noriman, Zulkepli, Dr.; Razif, Mohammad Nordin, Dr.; Sam, Sung Ting, Dr.; Mohd Mustafa Al-Bakri, Abdullah (AENSI Publisher All rights reserved, 2013-10)Cure characteristics and morphological studies were performed to determine the influences of TOR as a compatibilizer of styrene butadiene rubber/recycled chloroprene rubber (SBR/CRr) Blends. Both uncompatibilised and ... -
FT-IR and morphology of different recycled acrylonitrile-butadiene rubber glove (NBRgr) size and its blend ratios of SBR/NBRr blends
Nik Noriman, Zulkepli, Dr.; Lokman Hakim, Ibrahim; Rosniza, Hamzah; Mohd Arif Anuar, Mohd Salleh; Hanafi, Ismail; Sam, Sung Ting (Trans Tech Publications, Switzerland, 2012-12)Recycling rubber waste contributes to a cleaner environment by using indestructible rubber discards as well as lowering production costs as reclaimed rubber is cheaper than virgin or natural rubber. Therefore, in this ... -
The effects of tensile and morphological properties of Styrene Butadiene Rubber/Recycled Chloroprene Rubber (SBR/CRr) blends
Ahmad Azrem, Azmi; Nik Noriman, Zulkepli; Mohd Arif Anuar, Mohd Salleh; Razif, M.N. (Scientific.Net, 2012-12)The effects of tensile and morphological properties of styrene butadiene rubber/virgin chloroprene rubber blends (SBR/CRv) and styrene butadiene rubber/recycled chloroprene rubber blends (SBR/CRr) were investigated. The ...