High temperature corrosion behaviour of steel with a Carbonate deposit at 1123K
(2007)
The high temperature corrosion behavior of A1S1 304 austenitic stainless steel and S45C carbon steel were studied in presence with CaCO3 salt at 1123K for 24,48,72, 96 and 120 hour. The studies were carried out to determine ...
Hot corrosion behaviour of 18Cr-8Ni Austenitic Steel in presence of Na2S04 and transition metal salts
(The Japan Institute of Metals, 1984)
The high temperature oxidation behaviour of 18Cr-8Ni austenitic steel has been studied in presence of Na2S04 and transition metal salts, e.g. NiS04, CoS04, Cr2(S04)3, (NH4)2Mo04, NaV03 or Na2W04 in the temperature range ...
Oxidation behaviour of 18/8 Cr-Ni austenitic steel in presence of Na2SO4 and NiSO4 at 650 to 1000°C
(Carl Hanser Verlag, Germany, 1983)
Iron based alloys containing chromium as a major constituent with nickel additions are the most prominent materials in coal fired generating units and petroleum refinery plants. The corrosion of these alloys under service ...
Hot corrosion behaviour of Austenitic Steel-308 in Chloride salts
(2008)
The intensification of process engineering in almost every branch of modern technology, and development of new technologies make increasingly higher requirements for metallic construction materials, especially for their ...