Now showing items 1-9 of 9

    • High temperature corrosion behaviour of steel with a Carbonate deposit at 1123K 

      Habsah, Md Ishak; Mohammed Misbahul, Amin; Nazree, Derman; Khairul Rafezi, Ahmad (School of Materials Engineering, 2007)
      The high temperature corrosion behavior of A1S1 304 austenitic stainless steel and S45C carbon steel were studied in presence with CaCO3 salt at 1123K for 24,48,72, 96 and 120 hour. The studies were carried out to determine ...
    • Hot corrosion behaviour of 18Cr-8Ni Austenitic Steel in presence of Na2S04 and transition metal salts 

      A. U., Malik; Mohammed Misbahul, Amin; Sharif, Ahmad (The Japan Institute of MetalsChemistry Section, Z. H. College of Engineering and Technology, Aligarh Muslim University, 1984)
      The high temperature oxidation behaviour of 18Cr-8Ni austenitic steel has been studied in presence of Na2S04 and transition metal salts, e.g. NiS04, CoS04, Cr2(S04)3, (NH4)2Mo04, NaV03 or Na2W04 in the temperature range ...
    • Hot corrosion behaviour of Austenitic Steel-308 in Chloride salts 

      Mohammed Misbahul, Amin; Che Mohd Ruzaidi, Ghazali; Neelofar, Amin (School of Materials Engineering, 2008)
      The intensification of process engineering in almost every branch of modern technology, and development of new technologies make increasingly higher requirements for metallic construction materials, especially for their ...
    • The influence of different core arrangements on magnetic properties of electrical sheets under one-dimensional magnetizing system 

      Aisyah Hartini, Jahidin; Mahadi, W.N.L.W. (Institute of Electrical and Electronics Engineering (IEEE), 2007-12-06)
      This paper is concerned with the measurement on the magnetic properties of electrical steels under one-dimensional magnetizing system at the frequency of 50 Hz. The magnetic properties were principally investigated by ...
    • Oxidation behaviour of 18/8 Cr-Ni austenitic steel in presence of Na2SO4 and NiSO4 at 650 to 1000°C 

      Anees, Udin Malik; Mohammed Misbahul, Amin; Sharif, Ahmad (Carl Hanser Verlag, Germany, 1983)
      Iron based alloys containing chromium as a major constituent with nickel additions are the most prominent materials in coal fired generating units and petroleum refinery plants. The corrosion of these alloys under service ...
    • Oxidation behaviour of AISI-304 steel in the presence of Na2S04 and Fe2(S04)3 at 973 K 

      Mohammed Misbahul, Amin (Elsevier Science B.V., 1994)
      The high temperature oxidation behaviour of AISI-304 austenitic steel was studied in the presence of Na2S04, Fe2(S04)3 or a mixture at 973 K in flowing air. The studies were carried out to examine the influence of eutectic ...
    • Oxidation behaviour of low carbon steel in natural water 

      Mohammed Misbahul, Amin; W. B., Wan Nik; Kamaruzzaman, Yunus (Oriental Science Publishing CoFaculty of Science and Technology, University College of Science and Technology Malaysia, 2002)
      Natural water pollution has been identified as a potential danger to metallic materials used under service conditions. Sea water and lake water foulants have adequate corrosive environment due to chemical ingredients ...
    • Oxidation behaviour of mild steel in molten alkali metal salts deposits 

      Mohammed Misbahul, Amin; S., Hamdan; K., Ku Bulat (ASEAN Committee on Science & TechnologyDepartment Of Chemistry, Faculty Of Science And Technology, University College Of Science And Technology Malaysia, 2003-06)
      The oxidation behaviour of commercial mild steel has been investigated in presence of alkali metal salts viz. NaCl, Na2CC>3, KC1, K2CO3 in the temperature at 750°C for the period of 36 h in atmospheric condition. The low ...
    • The root caused analysis of leakaged heat exchanger tube 

      Shaiful Rizam, Shamsudin; Mohd Arif Anuar, Mohd Salleh; Azmi, Rahmat, Assoc. Prof. Dr.; Mazlee, Mohd Noor, Dr.; Mohd Harun; Hafizal, Yazid (Carl Hanser Verlag GmbH & Co., 2015-03)
      AISI type 316L stainless steel was used as a heat exchanger tube material in an inter-cooler column. After less than a year of operation, severe corrosion failures occurred and a transverse opening leakage was observed on ...