Hot corrosion behaviour of Nickel-200 alloy in presence of Sodium salts at 850°C
Abstract
The hot corrosion behaviour of Nickel-200 industrial alloy has been investigated in presence of Na2S04, NaCI, NaN03, Na2C03 and Na202 at 850°C in flowing air. The hot corrosion kinetic and effect of salt deposition on the corrosion rate were studied. The scale morphologies were determined on the basis of X-ray diffraction and Scanning electron microscopic techniques. It has been shown that an alloy corrodes at different rate in presence of different sodium salts although each salt contains the same amount of sodium equivalent to Na20.
Collections
Related items
Showing items related by title, author, creator and subject.
-
The effect of duration aging temperature on fatigue strength of aluminum alloy strength of aluminum alloy
Ahmad Syayuthi, Abdul Rahman; Haftirman; Teo, Ee Lynn (Universiti Malaysia Perlis (UniMAP)Pusat Pengajian Kejuruteraan Mekatronik, 2012-02-27)This paper present the effect of different duration aging temperature on fatigue strength of Al6063. Al 6063 alloy specimens have been solution heat treated at 520C for 2 hours. Subsequently, the artificial ageing heat ... -
Structural and phase formation of TiAl alloys synthesized by mechanical alloying and heat treatment
Al-Dabbagh, Jinan B.; Rozman, Mohd Tahar; Mahadzir, Ishak; Siti Aisyah, Harun (Universiti Malaysia Perlis, 2015)Mechanical alloying (MA) of Ti-50%Al (molar fraction) powder by using Planetary ball milling equipment, have been successfully refine the crystallite size and produced TiAl nano-alloys. The characteristics of the powder ... -
Preparation of submicron Al-Ti Alloy particles by mechanical alloying
Abdul Razak, Daud; Adolf Asih, Supriyanto (Universiti Malaysia Perlis, 2009-12-01)Introduction: Mechanical alloying (MA) is a solid-state powder processing technique involving repeated welding, fracturing and re-welding of powder particles in a high-energy ball mill [1-3]. MA has been used to synthesize ...