Show simple item record

dc.contributor.authorMohd Mustafa Al Bakri, Abdullah
dc.contributor.authorKamarudin, Hussin, Brig. Jen. Dato' Prof. Dr.
dc.contributor.authorKhairul Nizar, Ismail, Assoc. Prof. Dr.
dc.contributor.authorMohamed, Bnhussain, Prof. Dr.
dc.contributor.authorZarina, Yahya
dc.contributor.authorRafiza, Abdul Razak
dc.date.accessioned2013-08-14T14:29:47Z
dc.date.available2013-08-14T14:29:47Z
dc.date.issued2012
dc.identifier.citationAdvanced Materials Research, vol. 341-342, 2012, pages 189-193en_US
dc.identifier.issn1022-6680
dc.identifier.issn978-303785371-9
dc.identifier.issnhttp://www.scientific.net/AMR.341-342.189
dc.identifier.urihttp://dspace.unimap.edu.my/123456789/27445
dc.descriptionLink to publisher's homepage at http://www.ttp.net/en_US
dc.description.abstractGeopolymer requires an alkaline activator to induce it pozzolanic property and to accelerate the geopolymerisation process. The geopolymerisation process occurs due to the mixing of fly ash, sodium silicate and sodium hydroxide as the alkaline activator, which produces aluminosilicate gel that acts as a binder. As such, the ratios of fly ash to alkaline activator and Na 2SiO 3/NaOH play an important role in obtaining desirable compressive strength; the concentration of NaOH used in this study was 12 M. Different ratios of fly ash to alkaline activator (0.5, 1.0, 1.5, 2.0, 2.5 and 3.0) and Na 2SiO 3/NaOH (0.5, 1.0, 1.5, 2.0, 2.5 and 3.0) were investigated in order to determine the maximum compressive strength. The alkaline activator was mixed with fly ash with different ratio as mentioned above and the samples were cured at 70°C for 24 hours and tested on the seventh day. The maximum compressive strength was obtained when the ratios of fly ash to alkaline activator and Na 2SiO 3/NaOH were 2.0 and 2.5 with compressive strength 73.86 MPa.en_US
dc.language.isoenen_US
dc.publisherTrans Tech Publicationsen_US
dc.subjectCompressive strengthen_US
dc.subjectGeopolymeren_US
dc.subjectRatio fly ash to alkaline activatoren_US
dc.subjectRatio Na 2SiO 3/NaOHen_US
dc.titleCorrelation between Na 2SiO 3/NaOH ratio and fly ash/alkaline activator ratio to the strength of geopolymeren_US
dc.typeArticleen_US
dc.contributor.urlmustafa_albakri@unimap.edu.myen_US
dc.contributor.urlvc@unimap.edu.myen_US
dc.contributor.urlnizar@unimap.edu.myen_US
dc.contributor.urlbnhusain@kacst.edu.saen_US


Files in this item

Thumbnail

This item appears in the following Collection(s)

Show simple item record