Now showing items 1-6 of 6

    • Influence of polluted seawater on oxidation behaviour of Aluminum Alloy 

      Mohammed Misbahul, Amin; Ting, Tai Poh Yee; Ku Halim, Ku Bulat (Research Journal of Chemistry and Environment, 2005-12-24)
      Tropical harbors of Malaysia, the south china seawater characteristics have adequate corrosive environments due to chemical ingredients, biofouling nature as well as velocity. The influence of polluted seawater on oxidation ...
    • Influence of seawater pollution on corrosion of Iron-Carbon alloy 

      Mohammed Misbahul, Amin; Kamaruzzaman, Yunus; Ku Halim, Ku Bulat (Malaysian Society of Marines SciencesUniversity College of Science and Technology Malaysia, 2002-05-12)
      Seawater pollution has been identified as a potential danger to metallic materials used under service conditions. Seawater foulants have adequate corrosive environment due to chemical ingredients especially halides compounds. ...
    • Investigation of oxidative and corrossive inhibiting performance of vegetable oil 

      Wan Mohd Norsani, Wan Nik; Mohammed Misbahul, Amin; Ahmad, Jusoh; Noraaini, Ali (University College of Science and Technology MalaysiaFaculty of Science and Technology, 2004-05-31)
    • Low temperature oxidation behaviour of steel in molten alkali metal salts 

      Mohammed Misbahul, Amin (Kolej Universiti Sains dan Teknologi MalaysiaFakulti Sains dan Teknologi, Kolej Universiti Sains dan Teknologi Malaysia (KUSTEM), 2002-03-24)
    • Oxidation behavior of sensitized AISI 310 steel in KNO3 and K2CO3 at 1123 K 

      Mohd Misbahul, Amin, Assoc. Prof.; Che Mohd Ruzaidi, Ghazali, Assoc. Prof.; Amin, N. (The Minerals, Metals and Materials Society, 2009-12-07)
      Sometimes the operating temperature is such that the stainless steel can become sensitized, i.e. chromium carbide can precipitate at grain boundaries. The behavior of sensitized stainless steel is quite different from that ...
    • Water vapour effects on chromia forming alloys during cyclic oxidation 

      N.K., Othman; Azman, Jalar; N., Othman (Universiti Malaysia Perlis, 2009-12-01)
      Fe-Cr model alloys (Cr: 9, 17, and 25 wt %) were subjected to cyclic oxidation in Ar-20O2, Ar-20O2-5H2O and Ar-10H2-5H2O (pO2= 3.6 x 10-22 atm) all in volume % atmospheres at 700oC. In general, increasing alloy chromium ...