Show simple item record

dc.contributor.authorA., Ofiare
dc.contributor.authorS., Taking
dc.contributor.authorK., Karami
dc.contributor.authorA., Dhongde
dc.contributor.authorA., Al-Khalidi
dc.contributor.authorE., Wasige
dc.date.accessioned2022-05-09T04:19:37Z
dc.date.available2022-05-09T04:19:37Z
dc.date.issued2021-12
dc.identifier.citationInternational Journal of Nanoelectronics and Materials, vol.14 (Special Issue), 2021, pages 29-36en_US
dc.identifier.issn1985-5761 (Printed)
dc.identifier.issn1997-4434 (Online)
dc.identifier.urihttp://dspace.unimap.edu.my:80/xmlui/handle/123456789/75096
dc.descriptionLink to publisher's homepage at http://ijneam.unimap.edu.myen_US
dc.description.abstractIn this work, we report on the processing and device characteristics of AlGaN/GaN HEMT devices to investigate the effects of silicon dioxide (SiO2) etching using Fluoroform (CHF3) gas prior to gate metal deposition. Three different GaN device structures were fabricated: (a) device #1 in which the device passivation (using SiO2) and gate metallisation are done in one lithography step, (b) device #2 in which the device passivation and gate metallization are done in 2 separate steps, (c) device #3, in which the gate metallization is deposited prior to passivation. 100 nm of plasma enhanced chemical vapor deposition (PECVD) SiO2 was deposited for surface passivation to the devices. As fabricated, devices #1 and #2 exhibited very poor device characteristics with very low output currents which we attribute to surface plasma induced damage or changes on the gate region after the SiO2 etching. A two-step post gate annealing step was performed on the devices to recover this damage. The highest maximum drain current of over 1100 mA/mm was observed on device #3 after the first anneal step compared to other devices which showed higher maximum drain current after the second anneal step. All three devices show an improvement in self-heating behavior after the second anneal step along with more stable transfer characteristics. The highest maximum peak transconductance of over 250 mS/mm was observed on devices #2 and #3after the first anneal step. This reduces slightly for all devices but with more stable characteristics. The measured threshold voltage values (VTH) are also consistent and stable after performing the second anneal step. These results indicate that avoiding exposing the active region of GaN devices is important in achieving expected and stable characteristics. It also observed that further device improvement can be done by performing a two-step post gate annealing process.en_US
dc.language.isoenen_US
dc.publisherUniversiti Malaysia Perlis (UniMAP)en_US
dc.subject.otherAlGaN/GaNen_US
dc.subject.otherHigh electron mobility transistors (HEMTs)en_US
dc.subject.otherPlasma induced damageen_US
dc.subject.otherPost-gate annealingen_US
dc.titleInvestigation of plasma induced etch damage/changes in AlGaN/GaN HEMTsen_US