Study on solids-to-liquid and alkaline activator ratios on kaolin-based geopolymers
(Elsevier Ltd., 2012-10)
Kaolin and alkali activator were mixed with the solids-to-liquid ratios in range of 0.60-1.20 (Al 2O 3/Na 2O molar ratio of 0.63-1.27). Sodium silicate and sodium hydroxide ranged between 0.16 and 0.36 (SiO 2/Na 2O molar ...
Fly ash-based geopolymer lightweight concrete using foaming agent
(MDPI, Basel, Switzerland., 2012-06)
In this paper, we report the results of our investigation on the possibility of producing foam concrete by using a geopolymer system. Class C fly ash was mixed with an alkaline activator solution (a mixture of sodium ...