Self-compacting high density tungsten-bronze composites
(Elsevier, 2013-07)
Green compacts of W–bronze were encapsulated in shells of bronze powder, placed in a ceramic mold and sintered in alumina tube furnace at 1150 °C. Throughout the sintering cooling stage the differential coefficient of ...
Sintering behavior and microstructure evolution of mechanically alloyed W–bronze composite powders by two-step ball milling process
(Elsevier, 2013-01)
The miscibility of W in Sn and Cu is extremely poor. Sintering of W–bronze composites to their full density is proved to be difficult. To tackle this problem, the ball milling process of the W–bronze powder mixture proposed ...
Effect of different nickel content on the mechanical properties of hydroxyapatite-ni composites from coated powders
(Trans Tech Publications, 2014)
HA-Ni composites were fabricated by uniaxial pressing from coated powders, in which HA particles were successfully coated with nickel precursor by the electroless deposition method. The compacted powders sintered at ...
Sintering effects on mechanical properties of Co-HA composite prepared by modified electroless deposition.
(Trans Tech Publications, 2014)
Co-HA composite produced using electroless deposition without conventional sensitization and activation treatment was studied with varying sintering temperature (1100°C, 1200°C and 1250°C). The particles size, bulk density, ...