The influences of tor as a compatibilizer on cure characteristic and morphological properties of SBR/CRr blends
(AENSI Publisher All rights reserved, 2013-10)
Cure characteristics and morphological studies were performed to determine the influences of TOR as a compatibilizer of styrene butadiene rubber/recycled chloroprene rubber (SBR/CRr) Blends. Both uncompatibilised and ...
Preparation of cyciopentyi trisiianoi siisesquioxanes - modified natural rubber (CpSSQ(OH)3 - ENR-50) composite hybrid in the presence of HCI acid
(Trans Tech Publications, 2013)
A composite comprising cyclopentyl trisilanol siisesquioxanes (CpSSQ(OH)3) and 50% epoxidized natural rubber (ENR-50) was prepared at reflux temperature employed hydrochloric acid (HCl) as catalyst. HCl was found to be an ...
Green underfill - a novel green polymer hybrid as underfill material in electronic packaging application
(Macao Innovation & Invention Association, 2012-06-29)
Underfill is a material used to provide a stronger mechanical connection, provide heat bridge and to ensure the soldier joint are not stressed out due to differential heating on the chip and the rest of system.