Search
Now showing items 1-3 of 3
Oxidation behavior of AISI 304 steel in presence of Na2 SO4 and K2 SO4 at 900°C
(Carl Hanser Verlag, 1993)
Steels with high Cr- and Ni-contents utilized at elevated temperatures are oxidation resistant due to the formation of slowly growing, protective chromium oxide layers [1,2]. Na2SO4 or K2SO4 alone or in synergistic combination ...
Hot corrosion behaviour of Inconel-600 alloy in presence of NaCI and Na2CO3 at 850°C
(Carl Hanser Verlag, 1993)
Effect of Na2SO4 and Fe2(SO4)3 on the oxidation behaviour of AISI-303 Alloy at 900°
(Africa Journals Online, 1993)
The effects of NajS04 and Fe2(S04)3 coatings on the oxidation behaviour of AISI-303 alloy at 900° has been studied in flowing air. The coated samples were oxidised for a period up to 24 hr. The oxidation rate increased ...