dc.contributor.authorMohd Nazree, Derman-
dc.contributor.authorNormah, Che Man-
dc.date.accessioned2010-08-23T05:49:40Z-
dc.date.available2010-08-23T05:49:40Z-
dc.date.issued2010-06-09-
dc.identifier.citationp.165-169en_US
dc.identifier.isbn978-967-5760-02-0-
dc.identifier.urihttp://dspace.unimap.edu.my/123456789/9009-
dc.descriptionInternational Conference on X-Rays and Related Techniques in Research and Industry (ICXRI 2010) jointly organized by Universiti Malaysia Perlis (UniMAP) and X-Ray Application Malaysia Society (XAPP), 9th - 10th June 2010 at Aseania Resort Langkawi, Malaysiaen_US
dc.description.abstractThe corrosion behaviour of PM Al composite will be affected by the presence of alloying element and reinforcing phase in the composite. This study focused on magnesium and alumina Saffil™ short fibres reinforcement affected to corrosion behaviour of PM AMCs in 3.5wt% NaCl. PM Al composite and PM Al-Mg composite were fabricated from flaky aluminium powder, 2wt% granular magnesium and 15wt% alumina Saffil™ short fibres. The corrosion testing was done using potentiostat Gamry G300 to create Tafel plot and polarization curve. The corrosion effects were analyse using scanning electron microscopy (SEM) and X-ray diffraction analysis (XRD). From experiment, pitting was localized surrounding the magnesium constituents which occur randomly throughout the surface of PM Al-Mg composite. XRD analysis revealed that aluminum oxide (δ-Al Al1.67O4), aluminium hydroxide (Al (OH)3) and aluminium oxide (α-Al2O3) phases were detected in oxide film. The corrosion current density (Icrit) of PM Al composite is lower than PM Al-Mg composite which is 2.0 x 10-1 A/cm2 and 4.0 x10-1 A/cm2, respectively. Magnesium is used as inhibitor in corrosion behaviour of PM Al-Mg composite have been changed and protected with a stable formation of oxide film. The corrosion resistance of PM Al-composite was decreased with the presence of alumina Saffil™ short fibres in composite due to discontinuities in oxide film provided the corrosion initiated in sample.en_US
dc.language.isoenen_US
dc.publisherUniversiti Malaysia Perlisen_US
dc.relation.ispartofseriesProceedings of the International Conference on X-Rays & Related Techniques in Research & Industry (ICXRI2010)en_US
dc.subjectPowder metallurgyen_US
dc.subjectAluminiumen_US
dc.subjectMagnesiumen_US
dc.subjectCorrosion and compositeen_US
dc.subjectInternational Conference on X-Rays & Related Techniques in Research & Industry (ICXRI)en_US
dc.titleCorrosion behaviour of powder metallurgy aluminium matrix composite reinforced with alumina Saffil™ short fibreen_US
dc.typeArticleen_US
dc.publisher.departmentSchool of Materials Engineering & School of Environmental Engineeringen_US
dc.contributor.urlnazree@unimap.edu.myen_US
Appears in Collections:Conference Papers
Mohd Nazree Derman, Assoc. Prof. Dr.

Files in This Item:
File Description SizeFormat 
Corrosion Behaviour of Powder Metallurgy Aluminium Matrix Composite Reinforced with Alumina Saffil™ Short Fibre.pdfAccess is limited to UniMAP community659.99 kBAdobe PDFView/Open


Items in UniMAP Library Digital Repository are protected by copyright, with all rights reserved, unless otherwise indicated.