dc.description.abstractThis research was focused on the effect of sea mango fiber (SMF) content and chemical modification on tensile and thermal properties, morphology and moisture content of poly(vinyl alcohol) (PVA)/sea mango fiber (SMF) biocomposite films. The sea mango fiber filled poly (vinyl) alcohol biocomposite films were prepared by casting method at temperature 50°C for 24 hours. The biocomposite films were prepared with different SMF content from 0, 5, 10, 15 and 20 wt%. The result showed that the increasing SMF content has increased the tensile strength. The modulus of elasticity increased but the elongation at break decreases as the SMF content increased in PVA/SMF biocomposite films. The addition of SMF content also increased the moisture content of biocomposite films. The higher SMF content possessed better thermal stability. The scanning electron microscope (SEM) study was proven the poor interfacial adhesion between SMF and PVA matrix. The methyl methacrylate acid (MMA) was used as chemical modification. The chemical modification of SMF improved the properties of modified biocomposite films. The results indicates that the modified biocomposite films have higher tensile strength and modulus of elasticity but exhibit lower elongation at break compared to unmodified biocomposite films. The modified biocomposite films with MMA also lower the moisture content. The modified biocomposite films exhibits lower total weight loss at temperature 700°C compared to unmodified biocomposite films. The improved interfacial adhesion of modified PVA/SMF biocomposite films were proved by the morphological study. The FTIR showed the chemical modification of SMF with MMA reduced the hydroxyl group of SMF.en_US
dc.language.isoenen_US
dc.publisherUniversiti Malaysia Perlis (UniMAP)en_US
dc.subjectBiocomposite filmsen_US
dc.subjectCompositesen_US
dc.subjectSea mango fiber (SMF)en_US
dc.subjectFilleren_US
dc.subjectMatrixen_US
dc.subjectPoly(vinyl alcohol) (PVA)en_US
dc.titleProperties and characterization of cerber mangas (sea mango) filled poly (vinyl alcohol) biocomposite filmsen_US
dc.typeLearning Objecten_US
dc.contributor.advisorDr. Mohamad Syahmie Mohamad Rasidien_US
dc.publisher.departmentSchool of Materials Engineeringen_US
Appears in Collections:School of Materials Engineering (FYP)

Files in This Item:
File Description SizeFormat 
Abstract,Acknowledgement.pdf223.53 kBAdobe PDFView/Open
Introduction.pdf313.28 kBAdobe PDFView/Open
Literature Review.pdf456.62 kBAdobe PDFView/Open
Methodology.pdf430.51 kBAdobe PDFView/Open
Results and Discussion.pdf905.8 kBAdobe PDFView/Open
Conclusion and Recommendation.pdf195.82 kBAdobe PDFView/Open
Refference and Appendics.pdf347.94 kBAdobe PDFView/Open


Items in UniMAP Library Digital Repository are protected by copyright, with all rights reserved, unless otherwise indicated.