Please use this identifier to cite or link to this item: http://dspace.unimap.edu.my:80/xmlui/handle/123456789/33418
Full metadata record
DC FieldValueLanguage
dc.contributor.authorRohaya, Abdul Malek-
dc.contributor.authorYeoh, Chieh Hang-
dc.date.accessioned2014-04-03T14:30:33Z-
dc.date.available2014-04-03T14:30:33Z-
dc.date.issued2014-
dc.identifier.citationKey Engineering Materials, vol.594-595, 2014, pages 29-33en_US
dc.identifier.issn1662-9795-
dc.identifier.urihttp://dspace.unimap.edu.my:80/dspace/handle/123456789/33418-
dc.descriptionLink to publisher's homepage at http://www.ttp.net/en_US
dc.description.abstractA Co-Cr-Mo (ASTM CoF-75) alloy is normally used because of their good in physical, mechanical, wear and as well as biocompatibility. In order to obtain similarity chemical structure of bone, addition of HAP or TCP into CoF-75 alloy is required. The samples were fabricated using powder metallurgy (P/M) technique under pressure of 350 MPa and sintered at 1200 °C under argon atmosphere. The results on the effect of different additives were studied in terms of shrinkage, bulk density, apparent porosity and microstructural analysis.en_US
dc.language.isoenen_US
dc.publisherTrans Tech Publicationsen_US
dc.subjectCobalt-Chromium-Molybdenum (Co-Cr-Mo)en_US
dc.subjectHydroxyaapatite (HAP)en_US
dc.subjectPowder metallurgy techniqueen_US
dc.subjectTricalcium phosphate (TCP)en_US
dc.titleCharacterization of different additives of sintered cobalt F-75 alloy in biomaterial applicationsen_US
dc.typeArticleen_US
dc.identifier.urlhttp://www.scientific.net/KEM.594-595.29-
dc.identifier.doi10.4028/www.scientific.net/KEM.594-595.29-
dc.contributor.urlrohayamalek@unimap.edu.myen_US
dc.contributor.urljane2209@hotmail.comen_US
Appears in Collections:Rohaya Abdul Malek, Dr.
School of Materials Engineering (Articles)
Center of Excellence for Geopolymer and Green Technology (CEGEOGTECH) (Articles)



Items in UniMAP Library Digital Repository are protected by copyright, with all rights reserved, unless otherwise indicated.