Please use this identifier to cite or link to this item: http://dspace.unimap.edu.my:80/xmlui/handle/123456789/33289
Full metadata record
DC FieldValueLanguage
dc.contributor.authorMohd Irfan Hatim, Mohamed Dzahir, Dr.-
dc.contributor.authorUmi Fazara, Md. Ali, Dr.-
dc.contributor.authorMuhammad Syarhabil, Ahmad, Dr.-
dc.contributor.authorFahmi, Muhammad Ridwan, Dr.-
dc.date.accessioned2014-04-01T03:29:33Z-
dc.date.available2014-04-01T03:29:33Z-
dc.date.issued2013-
dc.identifier.citationProcedia Engineering, vol. 53, 2013, pages 71-80en_US
dc.identifier.isbn978-162748634-7-
dc.identifier.issn1877-7058-
dc.identifier.urihttp://www.sciencedirect.com/science/article/pii/S1877705813001318-
dc.identifier.urihttp://dspace.unimap.edu.my:80/dspace/handle/123456789/33289-
dc.descriptionLink to publisher's homepage at http://www.elsevier.com/en_US
dc.description.abstractA compact multifunctional Pd/alumina hollow fibre membrane reactor (HFMR) has been developed and used for the catalytic dehydrogenation of methylcyclohexane to toluene. The developed HFMR consists of a thin and defect-free Pd membrane of 5 um coated directly onto the outer surface of an alumina hollow fibre substrate. The substrate, was prepared by a phase inversion/sintering method, possess a unique asymmetric structure which can be characterised by a very porous inner surface from which finger-like voids extend across approximately 80 % of the fibre cross-section with the remaining 20 % consisting of a denser sponge-like outer layer. A 50 wt% Ni/Al2O 3 catalyst is directly deposited into the asymmetric support, with a fraction of catalyst particles distributed uniformly in the finger-like macro-voids while the others on the lumen surface forming a "filter- cake"-like layer. A significant increase in gas permeation resistance occurs due to this "filter-cake"-like catalyst layer when the catalyst loading (weight per unit fibre length) is above 2.3 mg-cm-1. Methylcyclohexane conversion increases with the increasing temperatures, because of the endothermic nature of the reaction; while decreases with the higher sweep gas flow rates due to the more serious catalyst deactivation in the HFMR. For a HFMR with 1.0 mgx-1 of catalyst loading, methylcyclohexane conversion of approximately 26% can be achieved at 610 °C with the sweep gas flowrate of 20 ml min-1, while for a porous membrane reactor and a fixed-bed reactor the methylcyclohexane conversion of 50% and 25% can be achieved at identical operating temperature.en_US
dc.language.isoenen_US
dc.publisherElsevier Ltd.en_US
dc.subjectAsymmetric structureen_US
dc.subjectCatalysten_US
dc.subjectMembrane reactoren_US
dc.subjectMethylcyclohexane dehydrogenationen_US
dc.subjectPd membraneen_US
dc.titleCatalytic dehydrogenation of methylcyclohexane (MCH) to toluene in a palladium/alumina hollow fibre membrane reactoren_US
dc.typeArticleen_US
dc.contributor.urlirfan@unimap.edu.myen_US
dc.contributor.urlumifazara@unimap.edu.myen_US
dc.contributor.urlsyarhabil@unimap.edu.myen_US
dc.contributor.urldrfahmi@unimap.edu.myen_US
Appears in Collections:Fahmi Muhammad Ridwan,Assoc. Prof. Dr.
School of Bioprocess Engineering (Articles)
School of Environmental Engineering (Articles)



Items in UniMAP Library Digital Repository are protected by copyright, with all rights reserved, unless otherwise indicated.