Please use this identifier to cite or link to this item: http://dspace.unimap.edu.my:80/xmlui/handle/123456789/28134
Title: Catalytic dehydrogenation of methylcyclohexane (MCH) to toluene in a palladium/alumina hollow fibre membrane reactor
Authors: Mohd Irfan Hatim, Mohamed Dzahir, Dr.
Umi Fazara, Md. Ali, Dr.
Muhammad Syarhabil, Ahmad, Dr.
Fahmi, Riduwan
irfan@unimap.edu.my
Keywords: Asymmetric structure
Methylcyclohexane dehydrogenation
Membrane reactor
PD membrane
Catalyst
Issue Date: 20-Nov-2012
Publisher: Malaysian Technical Universities Network (MTUN)
Citation: p. 421-428
Series/Report no.: Proceedings of the Malaysian Technical Universities Conference on Engineering and Technology (MUCET) 2012;
Abstract: A compact multifunctional Pd/alumina hollow fibre membrane reactor (HFMR) has been developed and used for the catalytic dehydrogenation of methylcyclohexane to toluene. The developed HFMR consists of a thin and defect-free Pd membrane of 5 μm coated directly onto the outer surface of an alumina hollow fibre substrate. The substrate, was prepared by a phase inversion/sintering method, possess a unique asymmetric structure which can be characterised by a very porous inner surface from which finger-like voids extend across approximately 80% of the fibre cross-section with the remaining 20% consisting of a denser sponge-like outer layer. A 50 wt% Ni/Al2O3 catalyst is directly deposited into the asymmetric support, with a fraction of catalyst particles distributed uniformly in the finger-like macro-voids while the others on the lumen surface forming a “filter-cake”-like layer. A significant increase in gas permeation resistance occurs due to this “filter-cake”-like catalyst layer when the catalyst loading (weight per unit fibre length) is above 2.3 mgcm-1. Methylcyclohexane conversion increases with the increasing temperatures, because of the endothermic nature of the reaction; while decreases with the higher sweep gas flow rates due to the more serious catalyst deactivation in the HFMR. For a HFMR with 1.0 mg cm-1 of catalyst loading, methylcyclohexane conversion of approximately 26% can be achieved at 610 °C with the sweep gas flowrate of 20 ml min-1, while for a porous membrane reactor and a fixed-bed reactor the methylcyclohexane conversion of 50% and 25% can be achieved at identical operating temperature.
Description: Malaysian Technical Universities Conference on Engineering and Technology (MUCET) 2012 organised by technical universities under the Malaysian Technical Universities Network (MTUN), 20th - 21st November 2012 at Hotel Seri Malaysia, Kangar, Perlis.
URI: http://dspace.unimap.edu.my/123456789/28134
Appears in Collections:Conference Papers
Umi Fazara Md. Ali, Assoc. Prof. Ir. Dr.
School of Environmental Engineering (Articles)

Files in This Item:
File Description SizeFormat 
CCE 14.pdfAccess is limited to UniMAP community 799.53 kBAdobe PDFView/Open


Items in UniMAP Library Digital Repository are protected by copyright, with all rights reserved, unless otherwise indicated.