Self-compacting high density tungsten-bronze composites
(Elsevier, 2013-07)
Green compacts of W–bronze were encapsulated in shells of bronze powder, placed in a ceramic mold and sintered in alumina tube furnace at 1150 °C. Throughout the sintering cooling stage the differential coefficient of ...
Sintering behavior and microstructure evolution of mechanically alloyed W–bronze composite powders by two-step ball milling process
(Elsevier, 2013-01)
The miscibility of W in Sn and Cu is extremely poor. Sintering of W–bronze composites to their full density is proved to be difficult. To tackle this problem, the ball milling process of the W–bronze powder mixture proposed ...