Characterization of cuprous oxide thin films on n-Si substrate prepared by sol-gel spin coating
(MASS Malaysia, 2008)
Cuprous oxide films were successfully grown onto a n-Si substrate with (100) orientation via sol-gel spin-coating method at room temperature in air followed by annealing in 5% H2 + 95% N2 atmosphere. The annealed temperatures ...
The effect of spin coating rate on morphology and optical properties of cuprous oxide thin film prepared by sol-gel technique
(Australian Ceramic Society, 2010)
Cuprous oxide thin films were successfully grown on indium tin oxide (ITO) coated glass by sol-gel spin coating using diethanolamine (DEA) as a solubility agent. The films were annealed at 350 °C in 5% H2 + 95% N 2 atmosphere. ...
Characterization of Cu2O thin films with addition of additive prepared by sol-gel spin coating process
(Universiti Putra Malaysia, 2010)
Cuprous Oxide (Cu2O) thin films were formed onto indium tin oxide (ITO) coated glass substrate by sol-gel spin coating technique using different additives namely polyethylene glycol and ethylene glycol. It was found that ...