Characterization of cuprous oxide thin films on n-Si substrate prepared by sol-gel spin coating
(MASS Malaysia, 2008)
Cuprous oxide films were successfully grown onto a n-Si substrate with (100) orientation via sol-gel spin-coating method at room temperature in air followed by annealing in 5% H2 + 95% N2 atmosphere. The annealed temperatures ...
Physical properties of cuprous oxide thin films grown on n-Si substrate by sol-gel spin coating
(Penerbit Universiti Kebangsaan Malaysia (UKM), 2009)
Cu2O films were grown on n-Si substrates via the sol-gel spin-coating method. The films were annealed under 5% H2 + 95% N2 atmosphere at 350°C, 450°C and 550°C. Diffractogram obtained by the grazing angle x-ray diffractometry ...