Search
Now showing items 1-5 of 5
High temperature corrosion behaviour of austenitic stainless steel with CaCO₃ and MgCO₃ deposit
(Universiti Malaysia Perlis (UniMAP), 2009)
The high temperature corrosion behaviour of austenitic stainless steel was studied at
850°C, 900°C, 950°C and 1000°C for 24 to 120 hr exposure time with CaCO₃ and
MgCO₃ deposit. Two commercial available austenitic stainless ...
Physical properties and corrosion behaviour of Co-Cr-Ni alloy developed by powder metallurgy
(Universiti Malaysia Perlis (UniMAP), 2011)
Cobalt-based alloys have been widely used in biomedical application. In this research, 11 different compositions of cobalt-chromium-nickel (Co-Cr-Ni) alloys were developed by powder metallurgy route. Scanning electron ...
The effect of HAP addition on properties F-75 alloy fabricated via P/M 6 for biomaterial applications
(Universiti Malaysia Perlis, 2010)
A Co-Cr-Mo (ASTM F-75) alloy is generally used because of their mechanical properties, good wear and corrosion resistance as well as biocompatibility. In order to obtain chemical similarity and interfacial bond form between ...
Corrosion behaviour on powder metallurgy aluminium matrix composite reinforced with alumina Saffil™ short fibres
(Universiti Malaysia Perlis, 2009)
The corrosion behaviour of PM Al composite will be affected by the presence of alloying element and
reinforcing phase in the composite. This studies were focused on the influence of magnesium addition
and alumina Saffil™ ...
Corrosion behaviour on AA2014/15vol. %A1₂0₃P and AA2009/20vol. %SiCw composite after ageing treatment
(Universiti Malaysia Perlis (UniMAP), 2007)
The purpose of this study is to compare the corrosion behaviour between AA2014/15vol. %A1₂0₃P and AA2009/20vol. %SiCw composites after ageing treatment. The former composite was cast composite supplied by Duralcan USA. The ...